...der bath temperature = 230c dipping time = 5 seconds the number of times = once use of r-type flux (2) use of sn-3.0ag-0.5cu solder bath solder bath temperature = 245c dipping time = 5 seconds the number of tim... |
Description |
4CH LOW INPUT ACTIVE HIGE−CURRENT DARLINGTON SINK DRIVER
|
File Size |
401.25K /
11 Page |
View
it Online |
Download Datasheet
|
|
|
 |
YAGEO Corporation
|
Part No. |
RC0100JR-070RL
|
OCR Text |
...free solder bath at 245 3 c dipping time: 3 0.5 seconds well tinned (> 95% covered) no visible damage -leaching ipc/jedec j-std-002b test d solder bath at 260 5 dipping time : 30 1 seconds no visible damage -resistance ... |